GGBS as a Partial Replacement of Cement in Concrete
Abstract
The rapid growth of infrastructure has increased the demand for concrete and, consequently, for cement. Cement production consumes considerable natural resources and contributes significantly to carbon dioxide emissions. Ground Granulated Blast Furnace Slag (GGBS), obtained from the iron One practical way of reducing this environmental impact is to replace a portion of cement with suitable industrial by-products.and steel industry, is one such material. Because its fineness and cementitious characteristics are suitable for use in concrete, GGBS has been widely studied as a partial cement replacement. This review discusses the production, physical and chemical properties, hydration behaviour, water absorption, and compressive strength of GGBS concrete. The reviewed studies generally show that GGBS can reduce the rate and peak of heat of hydration and can improve strength at later curing ages. Replacement levels in the range of about 30% to 60% can provide useful strength [d1 ,e2v, e5l]opment, although higher replacement levels may reduce early-age strength.
References
Reference [1] — Worrell et al. (2001), Carbon Dioxide Emissions from the Global Cement Industry
Used to support the environmental background: cement production contributes significantly to CO₂ emissions.
Provides the rationale for reducing ordinary Portland cement consumption. Reference [2] — Justnes (2015), How to Make Concrete More Sustainable
Used to introduce sustainable concrete and the use of supplementary cementitious materials. Supports the general argument that replacing part of cement can improve concrete sustainability.
Reference [3] — Pal, Mukherjee and Pathak (2003), Investigation of Hydraulic Activity of GGBS in Concrete Used to explain the hydraulic activity/reactivity of GGBS in cement-based concrete. Supports discussion of how GGBS contributes to cementitious reactions and strength development.
Reference [4] — Oner and Akyuz (2007), An Experimental Study on Optimum Usage of GGBS for the Compressive Strength of Concrete
Used for the relationship between GGBS replacement percentage and compressive strength. Supports discussion of selecting a suitable/optimum replacement level.
Reference [5] — Ozbay, Erdemir and Durmus (2016), Utilization and Efficiency of GGBS on Concrete Properties: A Review
Used as a broad review source for the effects of GGBS on concrete properties. Supports the summary of potential benefits and performance considerations.
Reference [6] — Barnett et al. (2006), Strength Development of Mortars Containing Ground Blast-Furnace Slag
Used for strength development at different curing temperatures and ages. Supports the explanation that curing conditions affect slag-containing mortar strength.
Reference [7] — Wang, Trettin and Rudert (2005), Effect of Fineness and Particle Size Distribution of Granulated Blast-Furnace Slag
Used to discuss how GGBS fineness and particle-size distribution affect hydraulic reactivity. Supports the statement that finer slag can react more readily, depending on its particle characteristics.
Reference [8] — Oner (2000), A Study of Intergrinding and Separate Grinding of Blast Furnace Slag Cement Used to discuss methods of grinding slag and cement. Supports the comparison between intergrinding and separate grinding for controlling blended cement properties.
Reference [9] — Islam et al. (1970), Strength Behavior of Mortar Using Slag as Partial Replacement of Cement
Used as supporting literature on strength when slag replaces a portion of cement in mortar. Relevant to the review’s discussion of mechanical performance of slag-based cement mixtures.
Reference [10] — Wang et al. (2018), Self-Hydration Characteristics of GGBFS by Wet-Grinding Treatment Used to discuss self-hydration/reactivity of GGBS and the influence of wet grinding
Refbacks
- There are currently no refbacks.